In plating a continuous strip of steel 0.9 m wide with Sn from an acid solution (valence charge=2), the desired strip speed is 500 m/min., current efficiency is 100%, and the thickness of tin plate is to be 0.4 μm (on each side) at a current density of 5000 A/m2. How long must the plating tank be assuming that the strip passes straight through the tank with no returns or bends? (density of Sn=7.31 g/cc, atomic weight of Sn=118.7).

ansver
Answers: 3

Another question on Engineering

question
Engineering, 04.07.2019 18:10
Give heat transfer applications for the following, (i) gas turbines (propulsion) ) gas turbines (power generation). (iii) steam turbines. (iv) combined heat and power (chp). (v) automotive engines
Answers: 1
question
Engineering, 04.07.2019 18:10
Slip occurs via two partial dislocations because of (a) the shorter path of the partial dislocation lines; (b) the lower energy state through partial dislocations; (c) the charge balance.
Answers: 1
question
Engineering, 04.07.2019 18:10
Which from the following instrument is commonly used to detect the high pitch butzing sound in bearings? [clo4] a)-digital ultrasonic meter b)-infrared camera c)-spectroscopic d)-vibrometer
Answers: 2
question
Engineering, 04.07.2019 18:20
Find the minimum film thickness for a journal bearing with the data below. shaft diameter, d-50 mm, clearance ratio, cdratio? 0.001, shaft speed, n 2000 rpm; bearing length. i 200 mm; eccentricity ration, ? -0.55. ( note, cdratio-ca/d) the minimum film thickness is um
Answers: 2
You know the right answer?
In plating a continuous strip of steel 0.9 m wide with Sn from an acid solution (valence charge=2),...
Questions
question
Mathematics, 27.06.2019 14:30
Questions on the website: 13722362